Effect of Hot-stamping on Microstructures and Tensile Properties of Al-Si Coated Boron Steel Welds with Laser Source
Myeong-Hwan Oh, Jong-Pan Kong, Min-Suck Kwon, Chung-Yun Kang
J Weld Join. 2013;31(6):96-106.   Published online January 21, 2014
PDFPDF    
2031558
Porosity Reduction in Laser Welding of Nitrided Carbon Steel
Young-Nam Ahn, Cheolhee Kim, Wonbeom Lee, Jeonhan Kim
J Weld Join. 2013;31(6):71-76.   Published online January 21, 2014
PDFPDF    
2031556
Laser Welding Characteristics of Aluminum and Copper Sheets for Lithium-ion Batteries
Minjung Kang, Taesoon Park, Cheolhee Kim, Jeonghan Kim
J Weld Join. 2013;31(6):58-64.   Published online January 21, 2014
PDFPDF    
Recent Study in Variation of Welding Materials for Overlay Welding
Ho-Cheon Yoo
J Weld Join. 2013;31(6):17-26.   Published online January 21, 2014
PDFPDF    
2031525
LIBS Analysis on Magnetic Force of Dissimilar Material Using SMAW
Chul Ku Lee, Wooram Lee
J Weld Join. 2013;31(4):54-61.   Published online August 31, 2013
PDFPDF    
2031520
Dual Laser Beam Joining Process for Polymers in Automotive Applications to Reduce Weights
Sang Bae Han, Hae Woon Choi
J Weld Join. 2013;31(4):23-27.   Published online August 31, 2013
PDFPDF    
2031519
Fiber Laser Welding in the Car Body Shop
- Laser Seam Stepper versus Remote Laser Welding -
Berthold Kessler
J Weld Join. 2013;31(4):17-22.   Published online August 31, 2013
PDFPDF    
2031518
Comparison of Powder Feeding and Wire Feeding in Laser Cladding
Young-Nam Ahn, Cheolhee Kim
J Weld Join. 2013;31(4):13-16.   Published online August 31, 2013
PDFPDF    
2031517
Effects of the Types of Coating on the Laser Brazing Characteristics of Dissimilar Joints between Mg Alloy and Steel Sheet
Mok-Young Lee, Sook-Whan Kim, ALI M. NASIRI, NORMAN Y. ZHOU
J Weld Join. 2013;31(4):7-12.   Published online August 31, 2013
PDFPDF    
2031516
Laser Stitch Welding Technology for the Fabrication of Automotive Parts
Sung-Min Joo, Hee-Seon Bang, Jun-Ui Han, Kyoung-Hak Kim, Byoung-Ho Ahn
J Weld Join. 2013;31(4):1-6.   Published online August 31, 2013
PDFPDF    
Effect of Coating Thickness on Microstructures and Tensile Properties in Yb:YAG Disk Laser Welds of Al-Si Coated Boron Steel
Wei-Ye Cao, Jong-Pan Kong, Yong-Nam Ahn, Cheol-Hee Kim, Chung-Yun Kang
J Weld Join. 2013;31(3):66-75.   Published online June 30, 2013
PDFPDF    
2031512
Characteristics of Plasma Emission Signals in Fiber Laser Welding of API Steel (Ⅲ)
Chang-Je Lee, Jong-Do Kim, Yu-Chan Kim
J Weld Join. 2013;31(3):60-65.   Published online June 30, 2013
PDFPDF    
The Weldability of the Dissimilar Magnesium Alloy Welded by Fiber Laser
Jong-Do Kim, Young-Sik Kim, Mook-Keun Song, Jung-Han Lee
J Weld Join. 2013;31(2):63-68.   Published online June 5, 2013
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI